In short

To protect face brick while retaining its appearance, identify the brick and finish, remove contamination and trial a suitable penetrating treatment on a discreet area. Brick varies in absorption, so a sample is essential. We check that the treatment is intended for the substrate and address joints or defects separately.

Check brick, mortar and exposure

Record whether the brick is new or older, its surface texture, any painted areas and the state of mortar joints. Check how the wall is exposed to rain and whether water collects at ledges, copings or window details. Different materials within one wall may absorb differently.

Look for loose mortar, cracking, salts or previous patching. Those conditions need evaluation before treatment, and new cement or masonry may have a product-specific maturity requirement. Do not apply a surface product over a wet, dirty or unsound area.

Inspect brick and mortar in both dry and damp conditions if the issue is rain entry. A treatment sample should be assessed after the product has dried as directed, but a sample does not prove that every part of a varied wall will look identical. Record which section was tested.

Identify the water problem

Water marks inside a face brick building may be caused by rain entry, a leaking roof, plumbing, condensation or ground moisture. The stain alone does not confirm that the brick needs sealing. Trace the likely water path and inspect nearby openings, joints and drainage.

Where water is entering through a crack or failed joint, repair that defect first. A repellent may be considered for suitable porous masonry, but it should not take the place of a repair or a designed waterproofing system.

Where previous patch repairs or repointing are visible, include them in the sample review. New mortar and older brick may absorb differently, and a uniform appearance should not be assumed. An applicator can help choose representative locations and explain what variation may remain.

Prepare a discreet sample

Choose a representative, inconspicuous location that includes the same brick and mortar condition as the main area. Clean and dry it using a method suited to the masonry, then follow the selected product instructions. Protect adjacent surfaces and let the sample dry as directed.

Assess the result in normal daylight and from the usual viewing distance. Check for changes in colour, sheen or patchiness. If the appearance is unacceptable or unclear, stop and seek advice rather than extending the treatment across the façade.

Check whether the wall needs cleaning and allow time to review the prepared surface. Cleaning can reveal colour differences that were hidden by dust or deposits. Agree that appearance before treatment is part of the approval, rather than asking the applicator to judge it alone.

Select treatment and application scope

SurfaPore C is described for porous concrete, masonry, stone and joints and does not form a surface film. SurfaPore FX WB is described for fragile mineral surfaces and preserving porosity, appearance and water-vapour permeability. We check each product against the brick condition and stated limitations.

A professional scope should include cleaning, repairs, sample approval, access, weather planning and records of treated elevations. Verify the current technical and safety data sheets, including surface and preparation instructions, before confirming the method.

If rain is entering at a window, coping or open joint, repair that detail before treating the brick face. Keep those items in separate lines of the work scope. This makes clear whether the proposal addresses absorption, a defect, or both. Follow the current technical and safety data sheets before application.

Plan a decision this week

If several units or a large wall are involved, agree the sample area with the body corporate or owner before work begins. Keep photographs and note the product and surface condition. This creates a reference point for the applicator and helps maintenance teams understand what was done.

This week, inspect one representative elevation, photograph the brick and joints, and ask an experienced applicator to prepare a small sample for review. Do not approve the full area until the appearance and scope have been discussed.

Questions

Will a clear treatment leave face brick unchanged?

No treatment should be assumed to leave every brick unchanged. Brick and mortar vary in absorption and appearance. We recommend a discreet sample, reviewed after drying in normal light, before approving work across a visible elevation.

Can face brick be treated if the mortar is cracked?

Cracked or loose mortar should be assessed and repaired as appropriate before a penetrating treatment is considered. A water repellent does not repair defective pointing or open joints, and the substrate must meet the selected product requirements.

Surface first

Tell us the surface and the problem. We send the right data sheets.

Send an enquiry
Ask about a surface